Basic Info
Specifications  of Suede PPGI

Base metalSuede PPGI
StandardASTM A653M/A924M 1998,JIS G3302,JIS G3312
GradeDX51D,SGCC,SPCC,SGCH
Thickness0.13-1.2mm
Width600-1250mm for Suede PPGI
Coil Weight3-8ton 
QualityDX51D Suede PPGI
Colorall RAL colors( standard international color) or customers samples color
Zinc Coating60-120g/m2
Coil ID508mm-610mm
Surface ProtectionPE,PVDF,SMP,HDP
Surface TreatmentChromate,oil/unoil,bright finish,spangle,anti-finger
Packingstandard export package
techniquecold rolled, hot-dipped galvanizing, color coated
paintingTop and bottom:20mic+5mic RMP     Back:6mic-8mic
toleranceThickness:+/-0.02mm
Width: +/-2mm

Applications  of Suede PPGI

ConstructionOutsideWorkshop, agricultural warehouse, residential precast unit, corrugated roof, roller shutter door, rainwater drainage pipe, retailer booth
InsideDoor, doorcase, light steel roof structure, folding screen, elevator, stairway, vent gutter
Electrical applianceRefrigerator, washer, switch cabinet, instrument cabinet, air conditioning, micro-wave oven, bread maker
FurnitureCentral heating slice, lampshade, chifforobe, desk, bed, locker, bookshelf
Carrying tradeExterior decoration of auto and train, clapboard, container, isolation lairage, isolation board
OthersWriting panel, garbage can, billboard, timekeeper, typewriter, instrument panel, weight sensor, photographic equipment

Structure Coating  of Suede PPGI

ItemThicknessTypeFeature for Suede PPGI
Laminated film50μmPolyethyleneProtecting from scratchs and contamination (option)
Top coat20μmPolyester FluorineChemical resistance and formability
Primer coat5μmPolyesterWorkability, corrosion resistance and adhesion to the primer coating
Chemical treatment1μmChromateGood adhesion and corrosion resistance
Substrate0.13mm-1.2mmGI.GL,ALGI.GL,AL
Back coat5±2μmEpoxyCorrosion resistance and adhesion to the substrate

Performance  Testing Of Suede PPGI

itemmethodconsequence
Tensile testTic-Tac-9mm 5mm cross cuppingNo damage
bending testT≤3No damage
boiling test100°C boiling 1 hourNo damage
Water resistance1000hours immersion in 40°C(edge)No damage
Moisture
 resistance
50°C90%100hours(edge)No damage
Brand NameSuede PPGISuede PPGI
Fire resistanceSamples were placed in incubators, remove greenhouse cooling, and then test the adhesionLong-term environment in 100°C
Fire extinctionLiquefied petroleum gas or natural gas burnerImmediately turn off
Drug resistance10%hydrochloric acid, saturated calcium,10%H2SO4,10%NAOH,gasoline,ethanolNo color and trace change
Salt spray test5%Nacl,35±2°C,500hoursNo damage

Coating  Performance test Standard Of Suede PPGI

Test itemPositive standardBack standard
Dry film thickness(um)14-167-9
Glass(60degree)High±5,Medium 40±5,low30±535±5degree
T bending33
Impact strength6.35.8
Pencil hardness(H)HH
MEK(Per)>100>100
Cross cut0 class0 class
Acid resistance50%H2SO4 immersion in300hrs,no color ,wrinkling, fading, change
Alkali resistance50%H2SO4 immersion in300hrs,no color ,wrinkling, fading, change
Aging-resistance1st class loss of color and glass
Salt spray500

Advantages Of Our  Suede PPGI
1. Resistance  to acid rain:
Coating protection mechanism: It is very easy to form acid rain in the high  level of industrial emissions or pollutants environment. Acidic penetration is  formed in the surface of pre-painted steel, and accelerates the corrosion,  forming blistering, peeling and so on.
2. Resistance  ultraviolet rays:
Coating protecting  Mechanism: pre-painted sheet in ultraviolet or strong sunlight conditions, the coating will exhibit chalking degeneration, manifested as discoloration and  loss of gloss, lose paint quickly.
3. Resistance to humid heat:
Coating protecting  mechanism: in hot and humid environments, high osmotic pressure of water vapor accelerates penetration, forming the degeneration of painting film, then the  corrosion of the substrate, with the phenomenon of bubbles and peeling.
4. Resistance to low temperature:
Coating protecting  mechanisms: most of the paint can keep stable processing performance above 0 degree, but at alpine region, the temperature will be below 20-40 degree,  normal paint will become brittle,bend cracking, or even lose paint, thus  protection function is lost totally.
FAQ
1.Are you a factory or a trading company?
Shandong Gengxiang Import and Export Trade Co.,Ltd is one of the leading China GI, GL, PPGI, PPGL manufacturers, and with professional factory we are able to provide you cheap GI, GL, PPGI, PPGL, galvalume steel coils with good quality
2.What's your MOQ?
 25MT, it is for one container.

3.What's your normal delivery time?
Our delivery time about 15-30days for standard sizes, if you have other requirements like hardness, quanity and width ,it is about 20-40days. But don't worry ,we also try our best for the delivery time ,because time longer and our cost is higher

 

Contact Us
Address: Room 1701, 2/F, Zhangdian Pancheng Trade Square, Zibo, Shandong Pr, China. (255000)
Tel: +86-533-6120355
 Fax:+86-533-3142961
 E-mail:Jennifer.jwj@Yahoo.com
Share: